Hi, I’ve tried to print a model plane for my father. It’s this model, using this LW-PLA right after purchase.
As you can see in the image of this post, the print is going well until it reaches a certain layer, where the filament does not get deposited properly for the entire layer, only intermittently. The following layers then, of course, have the same problem and I get this failed print with these “frayed ends”. Additional attempts failed the same way at a similar layer count.
If someone has some experience with lightweight PLA (LW-PLA) and knows what can be done to solve this, I and my father would greatly appreciate the help.
Thanks in advance.
Edit: Additional info: I’m using the PrusaSlicer files from the linked page. Edit2: The printer is Prusa Mk4.
It looks like there are multiple layers printed without feeding filament, which causes these frays to build up. Could it be that the filament clogs after this layer? Or do you see that filament still properly feeds later? This could happen for example due to heat creep and the filament getting too warm/soft in the extruder to properly feed or you trying to feed too fast.
Last time I tried, I think, I did multiple attempts back-to-back and starting again at layer 1 was no problem, so I don’t think it was clogged. I’ll experiment more with temperature and speed like you and others suggested.
It working again after cooling down is an indication for heat creep IMHO. The filament is getting too hot up to where the gears are, causing them to slip and not feed filament.
Oh, that makes sense. I’ll try with lower temperatures.